PROCEDE DE REDUCTION PAR FUSION DE MINERAI DE CHROME
| N° de brevet: |
EP0799899 (A1) |
| Date de publication: |
1997-10-08 |
| Inventeur(s): |
AIDA K [JP];TAKEUCHI S [JP];BESSHO N [JP];TERABATAKE T [JP];KISHIMOTO Y [JP];NISHIKAWA H [JP];SUDO FUMIO [JP]; |
| Demandeur(s): |
KAWASAKI STEEL CO [JP]; |
| Classification: |
C21C5/00;C21C5/35;C22B34/32; |
| N° de demande: |
EP19960932025 19960927 |
| Numéro(s) de priorité: |
WO1996JP02813 19960927;JP19950250826 19950928;JP19950324522 19951213 |
Résumé dans la langue de publication, traduction non disponible In this invention, the smelting reduction operation can be carried out in a high efficiency by charging a carbonaceous material in such an amount that total surface area is not less than 60 m**2 per 1 ton of slag weight. Furthermore, carbon substance finely particulating through thermal crumbling under a high-temperature atmosphere inside the vessel is used as the carbonaceous material, whereby it is possible to stably conduct the smelting reduction while controlling the scattering of the carbonaceous material, and also the erosion, particularly locally erosion of refractory in the smelting reduction furnace, which was a serious problem in the conventional technique, can considerably be decreased to largely prolong the service life of refractory.
|